Welding electrodes Monolith M-308L-16

AWS А5.4 / SFA-5.4: Е308 / Е308L-16
EN ISO 3581-А-E 19 9 L R 1 2
Terms of use
  • high welding and technological properties, low spatter, stable arc burning, easy slag removal, and excellent seam quality
  • excellent corrosion resistance in oxidizing environments and high resistance to intercrystalline corrosion
Special properties
  • type 302, 304 and 308 stainless steels
  • they are used for welding in all spatial positions, except vertical down one
  • welding is recommended to be performed at the highest possible speed without transverse oscillations of the electrode
Monolith M-308L electrodes are designed for welding of austenitic stainless steels such as 302, 304 and 308, etc. in the operating temperature range not exceeding 450°C (842°F). Main applications are found in equipment, tanks, cisterns and stainless steel pipes for use in the food, textile, oil refining, paper, and pharmaceutical industries, as well as in the automotive and general engineering industries.
Packaging data
Diameter, mm (in)Length, mm (in)Number of electrodes in a pack, pcs.Weight of the pack, kg (lb)
2,0 (5/64)300 (11,8)91 – 931 (2,2)
2,5 (3/32)350 (13,8)43 – 461 (2,2)
3,0 (1/8)350 (13,8)30 – 321 (2,2)
3,2 (1/8)350 (13,8)28 – 311 (2,2)
4,0 (3/16)350 (13,8)18 – 191 (2,2)

Monolith 308L-16 Ø2.5 (3/32); Ø 3.0 (1/8); Ø 3.2 (1/8) mm (in) are packed into a mini-tube of 3 pcs.

1 kg (2.2 lb) cardboard pack
20 packs per 20 kg (44 lb) cardboard box
50 cardboard boxes per 1 pallet
1000 kg (2200 lb) per 1 pallet
Coating type
rutile
CHEMICAL COMPOSITION OF DEPOSITED METAL, %
According to AWS A5.1 / Typical Results
C
Carbon
0.001
Mn
Manganese
0.86
Si
Silicon
0.71
P
Phosphorus
0.023
S
Sulfur
0.023
Cr
Chromium
19.57
Ni
Nickel
10.10
Mo
Molybdenum
0.018
Cu
Copper
0.05
WEDGE METAL MECHANICAL PROPERTIES
According to AWS A5.1 / Typical Results
  • Tensile strength, MPa 520 - 600 (75 - 87)
  • Yield point, MPa 370 - 490 (54 - 71)
  • Relative elongation, % 35 - 55
Baking before welding
  • the permissible moisture content in the coating before use is not more than 0.2 %;
  • if the electrode coating is moistened above normal, dry for 60 minutes at 400±10°С (752±50°F)
Welding modes
Welding current strength, A for electrodes with a diameter of, mm (in)
2.0 (5/64)2.5 (3/32)3.0 (1/8)3.2 (1/8)4.0 (5/32)
40 – 6060 – 9070 – 10080 – 11090 – 130